The graphite anode is used to electrolyze water solution to produce chlorine and caustic soda salt solution to produce caustic soda.
Chemical and physics properties of graphite anode
Item Grade | Resistivity μΩm | Ash % | Compressive Strength Mpa | Bending strength Mpa | Bulk Density g/cm3 |
First | 8 | 0.2 | 30 | 17 | 1.65 |
Second | 9 | 0.4 | 25 | 15 | 1.62 |
Specification of graphite anode
Types | Length mm | Wide mm | Depth mm | Angularity % | Weight kg |
Sy-6 | 760±5 | 85±1.5 | 40±1 | 1.5 | 4.5 |
Sy-7 | 760±5 | 180±1.5 | 40±1 | 1.5 | 9.2 |
Sy-8 | 760±5 | 180±1.5 | 40±1 | 1.5 | 9.0 |
Sy-9 | 960±5 | 180±1.5 | 40±1 | 2 | 11.2 |